GO-GREEN offers a complete range of lidding films that are engineered to work with the full spectrum of tray materials and for a complete range of applications. Optional printing is available in both flexo and roto gravure.

Availability
  • Fresh Wave Lidding Films - unique steam film.
  • Breathable OTR Specific Lidding Films - Fresh Produce and Seafood.
  • High Barrier Lidding Films - Ready Meals, Case Ready, High Pressure Pasteurization.
  • Lidding films with up to 11 layers for MAP have both easy peel and weld seal capabilities to PE, PP, PS, PE, Aluminum, CPET and PVC.



Downloads:
Lidding Summary Guide
Online Product Catalog

  Lidding Summary Guide
Lidding Gauge
Barrier
Anti Fog Sealing Max use* Min. use*
Substrate
 
Mil
 
AF
°C
°F
°F
PE
PP
PVC
PET
Al
PS
1
High Barrier
xx
120-150
185
0
weld
         
1.4
High Barrier
xx
100-180
208
0
weld
EP
       
HB 60(pdf)
2.4
High Barrier
xx
100-180
208
0
weld
EP
       
HB 80(pdf)
3.2
High Barrier
xx
100-180
208
0
weld
EP
       
 
2.4
Low Barrier
 
100-180
203
0
weld
EP
       
Breathable L 60**
2.4
Breathable
 
100-180
185
0
weld
EP
       
 
HB EP- A 62(pdf)
2.5
High Barrier
x
110-190
194
0
EP
         
HB EP-C 60(pdf)
2.4
High Barrier
 
140-200
257
0
weld
EP
EP
EP
 
EP
EP-C 42 (pdf)
1.7
Low Barrier
 
140-200
257
0
weld
EP
EP
EP
 
EP
 
L-PET 32(pdf)
1.3
Medium Barrier
             
weld
   
 
HB AL 50(pdf)
2
High Barrier
 
180-210
           
Hard peel
 
 
L PP 42(pdf)
1.7
Low Barrier
xx
130-190
212
0
 
weld
       
Breathable L PP 42**
1.7
Breathable
xx
130-190
212
0
 
weld
       
HB L PP 60(pdf)
2.4
High Barrier
xx
130-190
212
0
 
weld
       
 
FreshWave Steam Non-Barrier
(Microwave Only)
1.5 - 2.0
Breathable**
 
100- 180
300
0
 
weld
       
FreshWave Steam Airtight
(Microwave Only)
2.8 - 3.1
Barrier
 
150-210
300
0
 
weld
       


NOTE: Each application to be checked by customer.
* Maximum and minimum post treatment temperature or hot fill of package.
**Breathable OTR Specific films - contact your Go Green Sales Representative to define breathable target rates and to order test film.

Indicative OTR rates for High Barrier - 1 - 3 cc / m2 / day and Low Barrier - 100 cc / m2 / day(dry and 23°C). See link to data sheet for actual values.


Weld - Locked seal to tray
EP - Peelable Seal- (Harder Peel Strength can be sometimes achieved depending on sealing temp and dwell times.)